Design parameters: 1680KG of toluene, weight of material ((R)-4-chloro-3-trimethylsilyloxybutyronitrile): 500KG. Temperature ≤90℃, vacuum degree 0.09Mpa.
Advantages: The reactor of a company in Hunan volatilizes highly corrosive gases. Silicon carbide condensers were originally used for condensation and recovery. During operation, the silicon carbide condenser was damaged due to vibration, and the condenser often leaked. After the owner replaced the silicon carbide condenser with our company's perfluorinated condenser in early 2016, the condensation effect was improved. At present, the system has been running stably for more than 7 years.。